Polymer Property : Saybolt Viscosity at 100°F = 160 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 160 SUS
160 SUS
ChevronTexaco Transultex® CF G
Texaco Transultex CF metalworking fluids deliver value through:Excellent antiweld properties from active sulfur and chlorine-free EP compounding which reduce frictional heat, prevent welding of meta..
Saybolt Viscosity at 100°F 160 SUS
160 SUS
ConocoPhillips Hydroclear® 32 Multipurpose R&O Oil
Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidation inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear..
Saybolt Viscosity at 100°F 160 SUS
160 SUS
ConocoPhillips Hydroclear® 32 Ultra-clean multi-purpose R&O Oil
Description: Conoco Hydroclear Ultra-Clean Multipurpose R&O Oil is a rust- and oxidation-inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks..
Saybolt Viscosity at 100°F 160 SUS
160 SUS
ConocoPhillips Hydroclear® Heat Transfer Oil
Description: Conoco Hydroclear Heat Transfer Oil is a high-quality, thermally stable inhibited oil formulated from premium Conoco hydrocracked base stocks for use in heat-transfer service. Hydroclea..
Saybolt Viscosity at 100°F 160 SUS
160 SUS
ChevronTexaco Cleartex® D
Texaco Cleartex metalworking fluids deliver value through:Multipurpose performance — Texaco Cleartex cutting oils are tri-purpose, serving as the cutting oil, hydraulic fluid and machine lubricant ..