Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 1572 SUS | 1572 SUS | |
ChevronTexaco Clarity® ISO 320 Synthetic Paper Machine Oil FeaturesChevron Clarity Synthetic Paper Machine Oils combine the unique ashless formulation of Chevron Clarity® Paper Machine Oils with the superior performance properties of polyalphaolefin (PAO) .. |
|||
Saybolt Viscosity at 100°F | 1572 SUS | 1572 SUS | See Note 3. |
ChevronTexaco Marfak® Heavy Duty 2 Texaco Marfak grease delivers value through:Good film strengthGood rust and corrosion protection, even in wet conditions.Texaco Marfak greases are fibrous sodium soap greases. It resists oil separat.. |
|||
Saybolt Viscosity at 100°F | 1572 SUS | 1572 SUS | See Note 3. |
ChevronTexaco Marfak® Heavy Duty 3 Texaco Marfak grease delivers value through:Good film strengthGood rust and corrosion protection, even in wet conditions.Texaco Marfak greases are fibrous sodium soap greases. It resists oil separat.. |