Polymer Property : Oxygen Permeability = 72.26 cm3 mil/(100 in2 day atm) Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Permeability 1120 cm3 mil/(m2 day atm)
72.26 cm3 mil/(100 in2 day atm)
Topas Advanced Polymers TOPAS® 6013F-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6013F-04 is a high temperature, general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and p..