Polymer Property : API Gravity = 31.3 ° Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
API Gravity 31.3 °
31.3 °
ChevronTexaco Cleartex® CF F
Texaco Cleartex CF metalworking fluid delivers value through:Multipurpose performance — Texaco Cleartex CF metalworking fluid is tri-purpose - serving as the cutting oil, hydraulic fluid, and machi..
API Gravity 31.3 °
31.3 °
ChevronTexaco Gear Compounds EP, ISO 100
FeaturesChevron Gear Compounds EP are multipurpose gear lubricants.They provide good thermal stability, extreme pressure protection, antiwear and demulsibility, oxidation, rust, corrosion control an..
API Gravity 31.3 °
31.3 °
ChevronTexaco ISO 68 Utility Oil HVI
FeaturesChevron Utility Oil HVI is a high quality, high viscosity index uncompounded oil with excellent water separating characteristics.Chevron Utility Oil HVI possesses good natural thermal and ox..
API Gravity 31.3 °
31.3 °
ChevronTexaco ParaMount™ 3005 Paraffinic Process Oil
FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur..
API Gravity 31.3 °
31.3 °
ChevronTexaco Pinnacle® 680
Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o..
API Gravity 31.3 °
31.3 °
ChevronTexaco Syn-Star® GL SAE 80W-140
Texaco Syn-Star GL oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oil used in these products provides outstanding stability.Extended drain cap..
API Gravity 31.3 °
31.3 °
ChevronTexaco Torque Fluid
Chevron Torque Fluid is a high performance hydraulic fluid designed for use in transmissions and hydraulic systems requiring a fluid meeting the Allison C4 specificationIt is manufactured using high..
API Gravity 31.3 °
31.3 °
ConocoPhillips HD Fleet Supreme™ 15W-40 Engine Oil
Description: Conoco HD Fleet Supreme Engine Oil is a high-quality engine oil formulated from Conoco's premium hydrocracked base stock and unique additive technology. It easily satisfies the warr..
API Gravity 31.3 °
31.3 °
ChevronTexaco Canopus® 68
Texaco Canopus oils deliver value through:High resistance to forming emulsions due to excellent water separating characteristics.Long lubricant life provided by outstanding stability.Good lubricant ..