Polymer Property : API Gravity = 31.1 ° Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
API Gravity 31.1 °
31.1 °
15.6°C; ASTM D1298
ExxonMobil Teresstic 32
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
API Gravity 31.1 °
31.1 °
ChevronTexaco HDAX® ISO 68 NG Screw Compressor Oil
FeaturesChevron HDAX NG Screw Compressor Oils are formulated to meet the lubrication demands fo screw compressors in natural gas serviceprotect lubricated parts against the corrosive effects of wate..
API Gravity 31.1 °
31.1 °
ChevronTexaco Mechanism LPS® ISO 68 Hydraulic Oil
Chevron Mechanism LPS Hydraulic Oils are highly refined, paraffinic oils containing oxidation and rust inhibitors, and special antiwear additives to extend the life of hydraulic pumps and motor part..
API Gravity 31.1 °
31.1 °
ChevronTexaco Rando® HDZ 68
Texaco Rando HDZ oils deliver value through:High oxidation stability — Longer service life than attainable with conventional lubricants used in high pressure service.Protection against rust and cor..
API Gravity 31.1 °
31.1 °
15.6°C; ASTM D1298
ExxonMobil Teresstic 32
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
API Gravity 31.1 °
31.1 °
ChevronTexaco Cygnus® 100 Hydraulic Oil
Texaco Cygnus Hydraulic Oils deliver value through:High quality control — Enables customer to use lubricants almost as pure as the food being processedHigh performance — Provides lubrication bette..
API Gravity 31.1 °
31.1 °
ChevronTexaco Rykon® ISO 68 Premium Oil
FeaturesChevron Rykon Premium Oils are designed to give maximum protection to hydraulic pumps.They are formulated with ISOSYN® base stocks incorporating antiwear additives, oxidation and corrosion ..