Physical Properties | Metric | English | Comments |
---|---|---|---|
API Gravity | 30.6 ° | 30.6 ° | |
ChevronTexaco 600 White Oil FeaturesChevron Technical White Oils are high quality, highly refined, odorless, tasteless, clear, paraffinic, technical grade white oils.Chevron Technical White Oils are hydrocracked and dewaxed us.. |
|||
API Gravity | 30.6 ° | 30.6 ° | |
ChevronTexaco Delo® 400 SAE 10W Chevron Delo 400 heavy duty motor oils are exceptional, super premium quality “universal” engine oils which exceed industry and engine manufacturers’ performance requirements.They are formulated .. |
|||
API Gravity | 30.6 ° | 30.6 ° | |
ChevronTexaco Delo® 400 SAE 10W-30 Chevron Delo 400 heavy duty motor oils are exceptional, super premium quality “universal” engine oils which exceed industry and engine manufacturers’ performance requirements.They are formulated .. |
|||
API Gravity | 30.6 ° | 30.6 ° | |
ChevronTexaco Meropa® 100 Texaco Meropa oils deliver value through:Gear set efficiencies — High thermal stability EP system maintains clean gear and bearing surfaces, minimizing deposits which interfere with effective lubri.. |
|||
API Gravity | 30.6 ° | 30.6 ° | |
ChevronTexaco RPM® SAE 10W Heavy Duty Motor Oil Features: Chevron RPM Heavy Duty Motor Oils are premium quality, mixed fleet motor oils meeting the performance requirements of all four-stroke gasoline engines and all naturally aspirated, turbocha.. |
|||
API Gravity | 30.6 ° | 30.6 ° | |
ChevronTexaco Superla® 35 White Oil FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly ch.. |
|||
API Gravity | 30.6 ° | 30.6 ° | |
ChevronTexaco Superla® 38 White Oil FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly ch.. |
|||
API Gravity | 30.6 ° | 30.6 ° | |
ChevronTexaco URSA® SAE 10W Super Plus Texaco Ursa Super Plus oils deliver value through:Oil lasts longer between drains — Good oxidation stability protects against oil thickening during manufacturers recommended oil drain periods.Vital.. |
|||
API Gravity | 30.6 ° | 30.6 ° | |
ChevronTexaco ISO 100 Industrial Oil EP FeaturesChevron Industrial Oils EP are multipurpose oils for industrial service.Chevron Industrial Oils EP are designed to help minimize wear in all types of plant lubrication and also provide long .. |
|||
API Gravity | 30.6 ° | 30.6 ° | |
ChevronTexaco URSA® SAE 10W Extra Duty Texaco Ursa Extra Duty oils deliver value through:Excellent high temperature deposit control. Protects against high temperature oxidation and oil thickening.Special extreme pressure antiwear propert.. |