Physical Properties | Metric | English | Comments |
---|---|---|---|
API Gravity | 30.4 ° | 30.4 ° | |
ChevronTexaco 600R Neutral Oil FeaturesChevron Neutral Oils are all-hydroprocessed, highly refined API Group II paraffinic base stocks. Their extremely low sulfur, nitrogen, and aromatic content give them excellent thermal and o.. |
|||
API Gravity | 30.4 ° | 30.4 ° | |
ChevronTexaco Cleartex® E Texaco Cleartex metalworking fluids deliver value through:Multipurpose performance — Texaco Cleartex cutting oils are tri-purpose, serving as the cutting oil, hydraulic fluid and machine lubricant .. |
|||
API Gravity | 30.4 ° | 30.4 ° | |
ChevronTexaco Havoline® SAE 10W-30 Motor Oil All grades of Havoline Motor Oils are formulated with high quality base stocks, a shear-stable viscosity index improver, and contain detergent, dispersant, wear control, antioxidant, corrosion inhib.. |
|||
API Gravity | 30.4 ° | 30.4 ° | |
ChevronTexaco HDAX® SAE 15W-40 FeaturesChevron HDAX Ashless Gas Engine Oils are superior quality, ashless, gas engine oils.They are formulated with ISOSYN™ base stocks and a carefully balanced ashless package of dispersant, anti.. |
|||
API Gravity | 30.4 ° | 30.4 ° | |
ChevronTexaco ParaMount™ 6001 Paraffinic Process Oil FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur.. |
|||
API Gravity | 30.4 ° | 30.4 ° | |
ChevronTexaco RPM® SAE 10W-30 Heavy Duty Motor Oil Features: Chevron RPM Heavy Duty Motor Oils are premium quality, mixed fleet motor oils meeting the performance requirements of all four-stroke gasoline engines and all naturally aspirated, turbocha.. |
|||
API Gravity | 30.4 ° | 30.4 ° | |
ChevronTexaco Starguide™ ISO 150 Texaco Starguide oils deliver value through:Cleaner cutting — Reduce excessive drag that slows cutting.Exceptional performance for low water and low oil consumption saw systems.Excellent low temper.. |
|||
API Gravity | 30.4 ° | 30.4 ° | |
ChevronTexaco Superla® 50 White Oil FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly ch.. |
|||
API Gravity | 30.4 ° | 30.4 ° | |
ChevronTexaco Supreme SAE 10W-30 Motor Oil FeaturesChevron Supreme Motor Oils are premium quality automotive engine oils.Chevron Supreme Motor Oils SAE 5W-20, 5W-30, 10W-30, 10W-40, and 20W-50 are formulated with ISO-SYN™ base stocks, a she.. |
|||
API Gravity | 30.4 ° | 30.4 ° | |
ChevronTexaco Supreme SAE 10W-30 Synthetic Blend Motor Oil FeaturesChevron Supreme Synthetic Blend Motor Oil is premium quality automotive engine oil.It is formulated with a combination of synthetic and premium quality conventional base oils and specially s.. |
|||
API Gravity | 30.4 ° | 30.4 ° | |
ConocoPhillips Hydroclear® 15W-40 Power-D E.O. 15W-40 Description: Conoco Hydroclear Power-D Engine Oil, formulated from Conoco's premium hydrocracked base stock, protects diesel and gasoline engines against wear, deposits, varnish, rust and corros.. |
|||
API Gravity | 30.4 ° | 30.4 ° | |
ChevronTexaco Drive Train Fluid HD, SAE 10W FeaturesChevron Drive Train Fluids HD are high performance lubricants designed for use in transmissions, final drives, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or Allison C4 .. |
|||
API Gravity | 30.4 ° | 30.4 ° | |
ChevronTexaco URSA® SAE 10W-30 Super Plus Texaco Ursa Super Plus SAE 10W-30 delivers value through:One oil for all services, both diesel and gasoline, minimizes the chance of misapplication.Reduced inventory investment — No need to maintai.. |
|||
API Gravity | 30.4 ° | 30.4 ° | |
ConocoPhillips HD Fleet™ 30 Engine Oil Description: Conoco HD Fleet Engine Oil is a high-quality, single-grade oil formulated from Conoco's premium hydrocracked base stock and unique additive technology. This oil is highly recommende.. |
|||
API Gravity | 30.4 ° | 30.4 ° | |
ChevronTexaco SAE 10W Transmission and Drive Train TO-4 Oil Texaco Transmission and Drive Train TO-4 Oils deliver value through:Longer equipment life — Special additives protect metal surfaces against scuffing and wear even under severe operating conditions.. |