Physical Properties | Metric | English | Comments |
---|---|---|---|
API Gravity | 29.3 ° | 29.3 ° | |
ExxonMobil Mobil Clean 10W-40 Motor Oil Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes.. |
|||
API Gravity | 29.3 ° | 29.3 ° | |
ExxonMobil Mobil Pegasus 905 40 Mobil Pegasus 905 is an ultra-high performance gas engine oil engineered to meet the most rigorous demands of todays high output, low-emissions, fuel-efficient, four-cycle engines. These gas engines.. |
|||
API Gravity | 29.3 ° | 29.3 ° | 15.6°C; ASTM D1298 |
ExxonMobil Teresstic 68 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
API Gravity | 29.3 ° | 29.3 ° | |
ChevronTexaco 150 PMO ashless Texaco PMO Ashless oils deliver value through:High temperature stability — Contain an effective oxidation inhibitor to protect the oil at elevated ambient operating temperatures.Long lubricant life.. |
|||
API Gravity | 29.3 ° | 29.3 ° | |
ChevronTexaco Clarity® ISO 150 Paper Machine Oil FeaturesChevron Clarity Paper Machine Oils are the next generation circulating oils for the pulp and paper industry.Chevron Clarity Paper Machine Oils ISO 100, 150, and 220 are formulated with ISOS.. |
|||
API Gravity | 29.3 ° | 29.3 ° | |
ChevronTexaco ISO 150 Paper Machine Oil D FeaturesChevron Paper Machine Oils D are manufactured using select high viscosity index, paraffinic base stocks. Their additive packages include rust, oxidation, and foam inhibitors as well as an ef.. |
|||
API Gravity | 29.3 ° | 29.3 ° | |
ExxonMobil Mobil Clean 10W-40 Motor Oil Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes.. |
|||
API Gravity | 29.3 ° | 29.3 ° | |
ExxonMobil Mobil Pegasus 905 40 Mobil Pegasus 905 is an ultra-high performance gas engine oil engineered to meet the most rigorous demands of todays high output, low-emissions, fuel-efficient, four-cycle engines. These gas engines.. |
|||
API Gravity | 29.3 ° | 29.3 ° | 15.6°C; ASTM D1298 |
ExxonMobil Teresstic 68 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
API Gravity | 29.3 ° | 29.3 ° | |
ChevronTexaco Sultex® D Texaco Sultex delivers value through:Heavy duty performance — Texaco Sultex oils are designed for tough machining operations on difficult to machine metals and alloys.Low tool wear — Special compo.. |