Physical Properties Metric English Comments
API Gravity 26.6 °
26.6 °
ChevronTexaco Elite-Cut® NL Metal Working Fluid
FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met..
API Gravity 26.6 °
26.6 °
ChevronTexaco Taro® 16 XD SAE 50
Texaco Taro 16 XD delivers value through:Wear protection — Superior antiwear characteristics result in reduced wear on all moving engine components. Controls ring and liner wear through its ability..
API Gravity 26.6 °
26.6 °
ConocoPhillips 460 Bearing Oil
Description: Conoco Bearing Oil is formulated for the circulating systems that lubricate roll-neck bearings in steel and nonferrous rolling mills. It is suited for systems in which water and corrosi..