Physical Properties | Metric | English | Comments |
---|---|---|---|
API Gravity | 24.8 ° | 24.8 ° | |
ChevronTexaco ISO 680 Cylinder Oil W FeaturesChevron Cylinder Oils W are designed to meet the needs of emulsifying cylinder oils.Chevron Cylinder Oils W provide excellent metal wettability. The combination of oil emulsibility and metal.. |
|||
API Gravity | 24.8 ° | 24.8 ° | |
ChevronTexaco Vanguard® 680 Texaco Vanguard oils deliver value through:Excellent metal wettability and high film strength for any moisture condition.Versatility — Three viscosity grades available to cover the range of steam p.. |