Physical Properties | Metric | English | Comments |
---|---|---|---|
API Gravity | 24 ° | 24 ° | |
ChevronTexaco Delo® 2000 Marine Engine Oil, SAE 40 FeaturesChevron Marine Engine Oil Delo 2000 Marine is a high quality engine oil developed for use in a wide variety of medium speed trunk piston engines burning marine diesel oils, or residual fuels.. |
|||
API Gravity | 24 ° | 24 ° | |
ChevronTexaco ISO 32 Refrigeration Oil WF FeaturesChevron Refrigeration Oils WF are manufactured using medium viscosity index straight mineral oils. The base stocks are carefully selected to assure the low pour points that are necessary for.. |