Physical Properties | Metric | English | Comments |
---|---|---|---|
API Gravity | 22.8 ° | 22.8 ° | |
ChevronTexaco Elite-Cut® AD Metal Working Fluid FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met.. |
|||
API Gravity | 22.8 ° | 22.8 ° | |
ChevronTexaco ISO 100 Utility Oil LVI FeaturesChevron Utility Oils LVI are general purpose lubricants. Chevron Utility Oils LVI are light-colored oils that possess excellent natural low pour points, along with low carbon-forming tendenc.. |
|||
API Gravity | 22.8 ° | 22.8 ° | |
ChevronTexaco Biostar® Hydraulic 32 Texaco Biostar Hydraulic oils deliver value through:Environmental sensitivity — Readily biodegradable formulation supports use in environmentally sensitive applications.Reduced maintenance — Ashle.. |
|||
API Gravity | 22.8 ° | 22.8 ° | |
ChevronTexaco Alcaid® 100 Texaco Alcaid® oils deliver value through:Low pour points that permit oils to remain fluid at subzero temperatures.Ready separation from water, an important property where severe moisture condition.. |