Physical Properties | Metric | English | Comments |
---|---|---|---|
API Gravity | 22.7 ° | 22.7 ° | |
ChevronTexaco Extra Cutting Oil Texaco Extra Cutting Oil delivers value through:Excellent metal wetting and lubricity properties that allow the oil to spread rapidly on the metal surface and reduce friction and the chip-tool inter.. |
|||
API Gravity | 22.7 ° | 22.7 ° | |
ChevronTexaco ISO 100 Saw Guide Oil FeaturesChevron Saw Guide Oil is manufactured using naphthenic oils and specially selected additives
balanced to reduce friction between saw and guide components in thin kerf saw equipment. These ad.. |