Physical Properties | Metric | English | Comments |
---|---|---|---|
API Gravity | 20.9 ° | 20.9 ° | |
ChevronTexaco Cepheus® 150 Texaco Cepheus oil deliver value throughThe ability to retain lubrication properties in the presence of water.Good rust protection from a carefully designed additive package.The ease with which they.. |
|||
API Gravity | 20.9 ° | 20.9 ° | |
ChevronTexaco Elite-Cut® AXH Metal Working Fluid FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met.. |