Physical Properties | Metric | English | Comments |
---|---|---|---|
API Gravity | 20.5 ° | 20.5 ° | |
ChevronTexaco Cepheus® 220 Texaco Cepheus oil deliver value throughThe ability to retain lubrication properties in the presence of water.Good rust protection from a carefully designed additive package.The ease with which they.. |