Polymer Property : Oxidative Induction Time (OIT) = 75 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxidative Induction Time (OIT) 75 min
75 min
ASTM D3895
LyondellBasell Plexar® PX3216 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE
Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s..