Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxidative Induction Time (OIT) | >= 50.0 min @Temperature 210 - 210 °C |
>= 50.0 min @Temperature 410 - 410 °F |
Average value: 50.0 min Grade Count:1 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |