Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxidative Induction Time (OIT) | 32 min | 32 min | ISO 21809-1 |
Lushan PJ-1 Polypropylene Compounds for Steel Pipe Top Coats Polypropylene compound for steel pipe top coats Lushan PJ-1 is used for 3LPP coating system in colored white. It is supplied in pellets for melt extrusion or in a powder for application by spray or .. |