Polymer Property : Oxidative Induction Time (OIT) = 200 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxidative Induction Time (OIT) 10.0 - 200 min
10.0 - 200 min
Average value: 62.5 min Grade Count:4
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..