Physical Properties Metric English Comments
Oxidative Induction Time (OIT) 118 min
118 min
ASTM D3895
LyondellBasell Plexar® PX5335 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE
Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s..