Physical Properties | Metric | English | Comments |
---|---|---|---|
Pore Size | 250 - 4000 microns | 9.84 - 157 mil | |
FiberNide Nickel Foam Description: Produced in one meter wide continuous sheets in thickness from 1.6 to 2 mm and sold in rolls. Principally used to make the positive plate in nickel metal hydride batteries.Information .. |