Pore Size 0.00700 microns
0.000276 mil
Average Diameter
NanoScale NanoActive® Cerium Oxide
NanoActive CeO2 is produced using proprietary processes to obtain high specific surface area, aggregated dry powder that can be dispersed in various carrier fluids to significantly reduce the partic..