Pore Size 0.00430 microns
0.000169 mil
Median Pierce adsorption mesopore, based on surface area
Zircar Zirconia ZYBF-3 Zirconia Bulk Fiber Insulation
Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed ..
Pore Size 0.00430 microns
0.000169 mil
Median Pierce adsorption mesopore, based on surface area
Zircar Zirconia ZYBF-3 Zirconia Bulk Fiber Insulation
Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed ..