Physical Properties | Metric | English | Comments |
---|---|---|---|
Pore Size | 0.00270 microns | 0.000106 mil | Median Pierce adsorption mesopore, based on surface area |
Zircar Zirconia ZYBF-2 Zirconia Bulk Fiber Insulation Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed .. |
|||
Pore Size | 0.00270 microns | 0.000106 mil | Median Pierce adsorption mesopore, based on surface area |
Zircar Zirconia ZYBF-2 Zirconia Bulk Fiber Insulation Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed .. |