Polymer Property : Apparent Bulk Density = 1.60 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 1.60 g/cc
0.0579 lb/in³
Loose
CIMBAR BARIMITE™ NO. 22 Barites High Purity Barite (BaSO4)
Barimite Products are natural, off-white barites produced in Cartersville, Georgia. Cimbar's broad range of Barimite products are clean, high purity, high specific gravity, low solubility and chemi..
Apparent Bulk Density 1.60 g/cc
0.0579 lb/in³
Compacted
CIMBAR BARIMITE™ UF High Purity Barite (BaSO4)
Barimite Products are natural, off-white barites produced in Cartersville, Georgia. Cimbar's broad range of Barimite products are clean, high purity, high specific gravity, low solubility and chemi..
Apparent Bulk Density 1.60 g/cc
0.0579 lb/in³
Compacted
CIMBAR CIMBAR™ EX Barite Powder (BaSO4)
CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical ..
Apparent Bulk Density 1.60 g/cc
0.0579 lb/in³
Loose
CIMBAR CIMBAR™ PC Barite Powder (BaSO4)
CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical ..
Apparent Bulk Density 1.60 g/cc
0.0579 lb/in³
Compacted
CIMBAR CIMBAR™ UF Barite Powder (BaSO4)
CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical ..
Apparent Bulk Density 1.60 g/cc
0.0579 lb/in³
Loose
CIMBAR CIMBAR™ 325 Barite Powder (BaSO4)
CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical ..
Apparent Bulk Density 1.60 - 2.60 g/cc
0.0578 - 0.0939 lb/in³
Johnson Matthey Amoxis 10-1R N2O Abatement Catalyst
Odorless solid pellets, various dimensions. During the manufacture of Nitric Acid, significant quantities of pollutants are released into the atmosphere. One of the principal pollutants is the gree..