Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ISO 60 |
Hexion Bakelite™ 151733 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Contact strips.Information provided by Bak AGBak AG became a part of Hexion in 20.. |
|||
Apparent Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | Apparent density per ASTM D1895 |
Plenco 2424 Phenolic, Granular, Injection Molded
(discontinued **) Two-stage Phenolic. PLENCO 02424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a general purpose type material. It is used in electrical .. |
|||
Apparent Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D792 |
Covestro Baydur® 660 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Apparent Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D792 |
Covestro Baydur® 726 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Apparent Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D792 |
Covestro Baydur® 730 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Apparent Bulk Density | 0.640 - 0.700 g/cc | 0.0231 - 0.0253 lb/in³ | IS 867-1963 |
Amity Thermosets ATG 115 Phenolic Molding Organic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic .. |
|||
Apparent Bulk Density | 0.640 - 0.700 g/cc | 0.0231 - 0.0253 lb/in³ | IS 867-1963 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Compression Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications:Telecommuni.. |
|||
Apparent Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D4894 |
Solvay Specialty Polymers Algoflon® E2 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Pre Sintered. Type V Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent di.. |
|||
Apparent Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 6501 Phenolic Formaldehyde Resin, Low Shrinkage Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant.Application areas: Thermally and dyna.. |