Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.58 g/cc | 0.021 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Durez® 118 Phenolic, Compression Grade Durez 118 Black Phenolic is a two-stage, asbestos free, general purpose molding material. It exhibits improved impact strength and resistance to flexural fatigue for demanding automotive, electrica.. |