Polymer Property : Apparent Bulk Density = 0.490 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.490 - 0.510 g/cc
0.0177 - 0.0184 lb/in³
ASTM D792
LyondellBasell Montell HB312CM UHMW Polyethylene
Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transfer, ..
Apparent Bulk Density 0.490 - 0.510 g/cc
0.0177 - 0.0184 lb/in³
ASTM D792
LyondellBasell Montell HB320CM UHMW Polyethylene
Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transfer, ..
Apparent Bulk Density 0.490 g/cc
0.0177 lb/in³
ASTM D1895
Sumitomo Bakelite Durez® 31735 Phenolic, Compression Grade
Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension..
Apparent Bulk Density 0.490 g/cc
0.0177 lb/in³
ASTM D1895
Sumitomo Bakelite Durez® 31735 Phenolic, Injection Grade
Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension..
Apparent Bulk Density 0.490 g/cc
0.0177 lb/in³
Sumitomo Bakelite North America 2-530 Short-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Am..
Apparent Bulk Density 0.490 g/cc
0.0177 lb/in³
Arkema Group Lacovyl® GS 1300 PVC
LACOVYL GS 1300 is a vinyl chloride homopolymer produced by a suspension polymerization process.Characteristics : Viscosity index (ISO 1628-2):124 ml/g,(K value:70). Apparent density (ISO 60):0.49 g..