Physical Properties Metric English Comments
Apparent Bulk Density 0.440 g/cc
0.0159 lb/in³
Geon® 1169
PolyOne Geon™ 140 Series 140X484 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Shippin..
Apparent Bulk Density 0.440 g/cc
0.0159 lb/in³
Geon® STP 1169; Internal Method
PolyOne Geon™ Specialty Suspension Atlas E 43 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Atlas E 43 is a non-chain modified ultra-high molecular weight homopolymer specialty suspension resin intended for use in high strength extruded parts. It improves the physical properties, fo..
Apparent Bulk Density 0.440 g/cc
0.0159 lb/in³
ASTM D4894
Solvay Specialty Polymers Algoflon® F2 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope..