Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.390 - 0.770 g/cc | 0.0141 - 0.0278 lb/in³ | Average value: 0.603 g/cc Grade Count:11 |
Overview of materials for Polytetrafluoroethylene (PTFE), Conductive Carbon Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Conductive Carbon Filled". Each property range of values reported is min.. |
|||
Apparent Bulk Density | 0.390 g/cc | 0.0141 lb/in³ | ASTM D4894 |
Solvay Specialty Polymers Algoflon® 1.2CSC PTFE; Superconductive Carbon Filled
(discontinued **) Data provided by the manufacturer.1.2 wt.% Superconductive Carbon. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric prope.. |