Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.340 g/cc | 0.0123 lb/in³ | |
NanoAmor 95%, OD/WT/L: 40-70/5-30 nm/0.5-5 um Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |