Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.310 g/cc | 0.0112 lb/in³ | ASTM D4895 |
Solvay Specialty Polymers Algoflon® L203 Polytetrafluoroethylene (PTFE)
(Unverified Data**) Algoflon® L203 is a white PTFE micropowder comprising loose agglomerates of sub-micron sized particles. It is recommended for use as an additive in high quality oils and greases to reduce coefficie.. |