Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 1.56 g/cc | 0.0564 lb/in³ | |
Poco Graphite PYROGRAPH Ion Implant Grade Graphite Pyrograph is pyrolytically infiltrated graphite. POCO's proprietary process infiltrates the base material to a minimum depth of 0.1 inch throughout the entire surface of the component. This process .. |