Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Loose |
CIMBAR CIMBAR™ CF Barite Powder (BaSO4) CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical .. |