Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 1.02 g/cc | 0.0368 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Durez® 29502 Phenolic, Compression Grade Durez 29502 Brown Phenolic is a two stage, asbestos free, glass filled, special purpose molding material. It is formulated for close tolerance applications such as transmission valve bodies, and di.. |