Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.0210 g/cc | 0.000759 lb/in³ | On a discontinuous pre-expander |
Polimeri Europa Extir® EH 2000 Expandable Polystyrene Extir EH 2000 is an expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Extir EH 2000 is use.. |
|||
Apparent Bulk Density | 0.0210 g/cc | 0.000759 lb/in³ | On a continuous pre-expander after one expansion |
Polimeri Europa Extir Leonardo B 2000 AE Expandable Polystyrene
(discontinued **) Extir B 2000 AE is a flame retardant expandable polystyrene in the form of spherical beads of fine particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir B 200.. |
|||
Apparent Bulk Density | 0.0210 g/cc | 0.000759 lb/in³ | On a continuous pre-expander after one expansion |
Polimeri Europa Extir® E 5000 AE Expandable Polystyrene
(discontinued **) Extir E 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or H.. |
|||
Apparent Bulk Density | 0.0210 g/cc | 0.000759 lb/in³ | On a discontinuous pre-expander |
Polimeri Europa Extir® P 1212 Expandable Polystyrene
(discontinued **) Extir P 1212 is an expandable polystyrene in the form of spherical beads of very fine particle size and narrow distribution, containing pentane as blowing agent. Extir does not contain CFC or HCFC. .. |