Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | DIN 53 466 |
3M Dyneon™ TF 2029 PTFE Paste Extrusion Powder
(discontinued **) Type I PTFE. Free flowing powder. Minimum reduction ratio is 5; Max is 100. Average particle size 500 µm. Used for electrical insulating tapes, liners, and yarns.Dyneon offers a family of PTFE .. |
|||
Apparent Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | ASTM D1895 |
Plenco 7021 Black Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 7021 is the replacement material for the former Union Carbide BMRS-7021. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Apparent Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | ISO 60 |
SolVin 557RA Copolymer of Vinyl Chloride and Vinyl Acetate Made by suspension polymerization.
APPLICATIONS
Extrusion : sheets for vacuum-forming, for deformations of over 500 %
Calendering : rigid sheets for deep thermoformingInformation provided by SolVin... |
|||
Apparent Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | ASTM D792 |
Covestro Baydur® 660 IBS Polyurethane Structural Foam RIM, Density 30 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Apparent Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | ASTM D1895 |
ExxonMobil Paxon™ FD60-018 Compression Molding Resin FD60-018 is a very high molecular weight high density polyethylene powder. It exhibits very high impact strength.Information provided by ExxonMobil Chemical |
|||
Apparent Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | ASTM D1895 |
Plaslok 7021 Black Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 7021 is the replacement material for .. |