Physical Properties Metric English Comments
Apparent Bulk Density 0.460 g/cc
0.0166 lb/in³
ISO 60
Hexion Bakelite™ X30 Phenolic Formaldehyde Resin  (discontinued **)
Phenolic molding compound, reinforced with cotton and sisal fibers, increased notched impact strength.Application areas: Covers for electrical and electromagnetic devices.Information provided by Bak..
Apparent Bulk Density 0.460 g/cc
0.0166 lb/in³
MSZ ISO 60
BorsodChem ONGRO CPE 3602 C Chlorinated Polyethylene
IMPACT MODIFIER FOR PVChigh impact resistancegood processabilityexcellent weather resistanceELASTOMERSvariety of cross-linking technologiesexcellent ozone- and weather resistanceexcellent chemical r..