Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.430 g/cc | 0.0155 lb/in³ | Geon® STP 1169; Internal Method |
PolyOne Geon™ 210 Series 215 Blending Resin Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 215 is a low molecular weight particle size homopolymer blending resin intended for use in plastisol formulations. It improves air release performance resulting in reduced scrap rates. It dec.. |
|||
Apparent Bulk Density | 0.430 g/cc | 0.0155 lb/in³ | ASTM D4894 |
Solvay Specialty Polymers Algoflon® 25CAR+5CER PTFE; Petroleum Coke and Ceramic Filled
(discontinued **) Data provided by the manufacturer.25 wt.% Petroleum Coke + 5 wt.% Ceramic. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectr.. |
|||
Apparent Bulk Density | 0.430 g/cc | 0.0155 lb/in³ | ASTM D4894 |
Solvay Specialty Polymers Algoflon® 25CAR PTFE; Petroleum Coke and Graphite
(discontinued **) Data provided by the manufacturer.25 wt.% Petroleum Coke and Graphite. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric p.. |