Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.350 g/cc | 0.0126 lb/in³ | ASTM D4895 |
Solvay Specialty Polymers Algoflon® L100 Polytetrafluoroethylene (PTFE)
(Unverified Data**) Algoflon® L100 is a white PTFE micropowder comprising loose agglomerates of sub-micron sized particles. Algoflon® L100 is specially polymerized to obtain a powder with exceptionally high specific .. |