Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.0110 g/cc | 0.000397 lb/in³ | On a continuous pre-expander after two expansions |
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene
(discontinued **) Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |