Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.0600 - 0.0800 g/cc | 0.00217 - 0.00289 lb/in³ | |
NanoAmor 95%; OD: 80-200 nm Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Apparent Bulk Density | 0.0600 - 0.0800 g/cc | 0.00217 - 0.00289 lb/in³ | |
NanoAmor 99.8%; OD: 80-200 nm Graphitized Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |