Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.0560 g/cc | 0.00202 lb/in³ | Free-rise Density, Bayer test |
Covestro Bayfill® 310 Polyurethane Semi-Rigid Foam, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |