Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.0500 g/cc | 0.00181 lb/in³ | |
NanoAmor 95%, OD/ID: < 8/2-5 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Apparent Bulk Density | 0.0500 g/cc | 0.00181 lb/in³ | |
NanoAmor 95%, OD/ID: 8-15/3-5 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |