Physical Properties Metric English Comments
Apparent Bulk Density 0.0200 g/cc
0.000723 lb/in³
On a discontinuous pre-expander
Polimeri Europa Extir® F 1111 Expandable Polystyrene  (discontinued **)
Extir F 1111 is an expandable polystyrene in the form of spherical beads of very fine particle size and a narrow particle size distribution, containing pentane as blowing agent. Extir does not cont..