Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Apparent Bulk Density = 0.000578 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.0160 g/cc
0.000578 lb/in³
On a continuous pre-expander after one expansion
Polimeri Europa Extir® LN 3000 Expandable Polystyrene
Extir LN 3000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion..
Apparent Bulk Density 0.0160 g/cc
0.000578 lb/in³
On a discontinuous pre-expander
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene  (discontinued **)
Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or CFC. Extir D 30..
Apparent Bulk Density 0.0160 g/cc
0.000578 lb/in³
On a continuous pre-expander after one expansion
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene  (discontinued **)
Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext..
Apparent Bulk Density 0.0160 g/cc
0.000578 lb/in³
On a discontinuous pre-expander
Polimeri Europa Extir® E 5000 AE Expandable Polystyrene  (discontinued **)
Extir E 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or H..
Apparent Bulk Density 0.0160 g/cc
0.000578 lb/in³
On a continuous pre-expander after two expansions
Polimeri Europa Extir® EH 5000 Expandable Polystyrene
Extir EH 5000 is an expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. This grade i..
Apparent Bulk Density 0.0160 g/cc
0.000578 lb/in³
On a discontinuous pre-expander
Polimeri Europa Extir® LN 2000 Expandable Polystyrene
Extir LN 2000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion..