Physical Properties | Metric | English | Comments |
---|---|---|---|
Grain Size | 800 - 1000 µm | 800 - 1000 µm | |
Sharadaa Ceramics Calcium Silicate Block Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |