Physical Properties | Metric | English | Comments |
---|---|---|---|
Grain Size | 1.0 µm | 1.0 µm | Median |
Nabaltec NABALOX® NO 613-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Grain Size | 1.0 - 2.0 µm | 1.0 - 2.0 µm | |
Inhance Fluoro-Seal INHANCE® Ti--9113 Titanium Carbide Polymer Alloy Product Description: INHANCE Ti-9113 polymer alloy consists of spherically shaped titanium carbide micro grains chemically bonded to surface-activated Ultra High Molecular Weight Polyethylene (UHMW.. |