Physical Properties | Metric | English | Comments |
---|---|---|---|
Grain Size | 0.80 µm | 0.80 µm | Median |
Nabaltec NABALOX® NO 713-10 MF Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Grain Size | 0.80 µm | 0.80 µm | Median |
Nabaltec NABALOX® NO 713-10 RF Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |