Polymer Property : Viscosity = 990 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 990 cP
990 cP
BASF Lupranate® 279 Isocyanate
Description: Lupranate® 279 Isocyanate is a 14% free-NCO prepolymer based on monomeric MDI chemistry. Lupranate 279 Isocyanate provides the lengthened open-time and high elongation desired in appli..